Atomic H from corrosion or cathodic-charge enters metal lattice and reduces toughness; high-strength steels (above 1000 MPa) and Ti alloys vulnerable; trapped at dislocations and grain boundaries.
Atomic H from corrosion or cathodic-charge enters metal lattice and reduces toughness; high-strength steels (above 1000 MPa) and Ti alloys vulnerable; trapped at dislocations and grain boundaries.